Mixing | Use the power mixer to mix the main paint evenly, and then as you stir it, you add the hardener until you get to mix well. Generally, if the temperature below 10 ℃, it needs 30 min induction time; if the temperature over 10℃, it needs 15 min induction time. |
Thinner | Epoxy paint thinner |
Mixing ratio | Part A: Part B = 24:4 |
Airless spray | Nozzle tip: 0.018~0.027inches Spray pressure: 15~18Mpa Thinner ratio: 5~15% (by weight of paint) |
Brush, Roller | Recommended Must achieve required thickness. |
Substrate Temperature | 10 ℃ | 20 ℃ | 30 ℃ |
To touch(75um) | 4h | 2h | 1h |
To handle(75um) | 48h | 24h | 16h |
Min. recoating time | 56h | 6h | 4h |
Max. recoating time | 60d | 30d | 30d |
Pot life | 6h | 4h | 2h |
* Make sure no chalking and other contaminations before recoating. If necessary, stucco thoroughly before coating.
* Above data for reference only, actual drying time and recoating time is dependent on temperature, dry film thickness, ventilation conditions, humidity, mechanical strength, etc.
Color | Gray, Bronzing |
Gloss | Flat |
Density | ~1.6Kg/L(after mixing) |
Hardness | Curing agent for epoxy paint |
Solid Volume | (75±2 )% |
Standard Film thickness | 150um dry film thickness (about 200um wet film thickness) |
Theoretical spreading rate | 3.13m²/Kg (150um dry film thickness) |
Full cure | (23±2℃) 7d |
Flash point | 39℃ |