Most colored quartz floors that fail in their first two years were not let down by the resin. They were let down by a slab nobody tested, a dew point nobody checked, or a batch left too long in the pail.
Epoxy colored sand flooring — graded colored quartz bound in clear epoxy — gives a seamless, high-wear, chemical-resistant finish for food plants, healthcare, retail and parking decks. It is also among the least forgiving systems to install. Here is the commercial sequence, from survey to handover.
Two systems share the name, and their numbers are not interchangeable. Compacted or trowel-applied quartz is built at 3–5 mm, spread by screed and densified with a power trowel before sealing — the heavy-traffic option. Self-leveling colored sand is placed at roughly 1.5–2 mm, poured in ribbons, gauge-raked and spike-rolled. Coverage, working time and cure schedules can differ twofold. Pull the TDS for the exact SKU on the pallet, not the family brochure, and set quantities, crew and programme from it. If the TDS and site conditions disagree, settle it before a kit is opened.
Indicative ranges from published manufacturer data; your own TDS governs.
|
Check |
Typical published reference |
|
Ambient and substrate temperature |
10–30 °C (some systems 5–35 °C) |
|
Relative humidity |
≤ 75–85% |
|
Substrate moisture content |
≤ 6–8% |
|
Substrate temperature above dew point |
≥ 3 °C |
|
Concrete compressive strength |
≥ 25 MPa, or C25 and above |
Log the readings, not just the passes. Walk the slab for oil, curing compound, laitance, old coatings, active cracks and movement joints. Damp-proof membranes, covings and hygiene detailing belong in this survey, not in a change order. Honour structural joints through the full build-up: seamless never means bridging a moving joint.
Grind or shot-blast to the TDS profile, often a uniform 60-grit-like texture. Remove laitance, sealers and contaminants, degrease oil, and extract dust with an industrial vacuum, never a broom. Repair cracks and divots with compatible epoxy mortar and let it cure — silicone fillers destroy adhesion. Re-check flatness: colored sand follows the slab, it does not hide a bad one. Residual dust becomes a bond-line release agent.
Mix primer at the stated ratio and apply evenly at TDS coverage. It wets the pores, cuts outgassing bubbles and evens out suction. Watch absorbent patches — a starving primer reads later as dull spots and shade variation. Respect the recoat window; fully cured primer may need light abrasion.
Work in continuous bays with a planned wet edge. Compacted systems: spread to build, then densify with a power trowel until voids close. Self-leveling grades: pour in ribbons, gauge-rake, spike-roll immediately — once the material gels, the roller leaves permanent tracks. Plan terminations and covings before the first batch; a gelled bay cannot be joined invisibly. Use one aggregate lot and consistent trowel pressure, or shade banding will be read as a color fault. Exclude dust, water and traffic throughout.
The quartz layer is porous by design. After the stated interval — often around 24 hours — apply the seal coat to fill the interstices. That is what makes the floor cleanable, non-shedding and chemically resistant. Wet or hygiene-critical areas commonly take a second seal or a wear-resistant topcoat. Confirm slip rating and gloss with the client first; both are decided here.
Indicative reference times, subject to the TDS:
|
Stage |
Typical reference |
|
Surface dry |
4–8 hours |
|
Light foot traffic |
24–48 hours |
|
Vehicle and heavy traffic |
Around 72 hours |
|
Full chemical cure |
Approximately 7 days |
Barricade the area and ventilate without directing dust-laden air across the surface. Keep water, spills and loads off until full cure. Hand over cleaning instructions: neutral-pH cleaners, no aggressive pads early on.
|
Symptom |
Most likely cause |
|
Blisters or pinholes |
Outgassing from a damp slab, thin primer, late spike rolling |
|
Delamination |
Weak profile, laitance, dust, moisture, missed recoat window |
|
Shade banding |
Mixed aggregate lots, uneven trowel density, inconsistent mixing |
|
Whitening or amine blush |
High humidity, cold cure, condensation before sealing |
|
Soft or tacky patches |
Off-ratio mixing, unmixed material from the pail, cold substrate |
|
Slow cure |
Low temperature, excessive build, incorrect hardener |
Can it go over an existing coating? Only after adhesion testing and removal of anything unsound. Grinding back to sound concrete is usually cheaper than remediation.
How thick should the build be? Match the traffic class: roughly 1.5–2 mm for self-leveling grades, 3–5 mm for compacted quartz, per the selected TDS.
When can the client wash the floor? Light cleaning once the seal coat has cured; no wet washing or chemical exposure before full cure.
A colored quartz floor is not finished when it looks dry. It is finished when the slab, the batch and the cure schedule all agree with the data sheet.