Mixing | Use the power mixer to mix the main paint evenly, and then as you stir it, you add the hardener until you to mix the paint well. |
Mixing Ratio | Part A: Part B= 5:1 (by weight) |
Thinner | Exclusive thinner |
Airless spray | Nozzle tip:0.018~0.025inch Spray pressure:18~25MPa Thinner ratio:5~15% (by weight of paint) |
Brush、Roller | Recommended for small areas only. Must achieve required thickness |
Substrate Temperature | 10 ℃ | 20 ℃ | 30 ℃ |
To touch(30um) | 8h | 4h | 3h |
To handle(30um) | 36h | 24h | 24h |
Min. recoating time | 16h | 4h | 3h |
Max. recoating time | 10d | 7d | 5d |
Pot life | 6h | 4h | 2h |
* Make sure no chalking and other contaminations before recoating.
* Above data for reference only, actual drying time and recoating time is dependent on temperature, dry film thickness, ventilation conditions,humidity, mechanical strength, etc.
Color | Light Gray |
Gloss | Matt |
Density | -1.32Kg/L |
Hardeness | Epoxy curing agent |
Solid Volume | (45±2 )% |
Standard Film thickness | 60µm dry film thickness (about 135µm wet film thickness) |
Theoretical spreading rate | 5.68m²/Kg(60µm dry film thickness) |
Full cure | (23±2℃) 24h |
Flash point | 27℃ |